Material Notes:
Information provided by Reliance Industries
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
Flexural Strength 46.0 MPa
6670 psi
Flexural Modulus <= 4.10 GPa
<= 595 ksi
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F