Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOTAL Petrochemicals Polypropylene 4252 is a 1.5 melt flow rate impact copolymer designed for improved toughness and high melt strength. This resin offers outstanding processability in combination with excellent mechanical properties. Total polypropylene 4252 was specifically developed for the extruded cardboard market.High Purity. Low catalyst residues in TOTAL Polypropylene 4252 allow extended processing runs without screen pack pluggage.FDA. 4252 complies with all applicable FDA regulations for food contact applicationsRecommended Applications. 4252 is recommended for corrugated sheet, profile extrusion, blow molding, thermoforming and slit film for carpet backing applications.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 6.5 %
6.5 %
ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Pressure unspecified; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 204 - 260 °C
400 - 500 °F