Material Notes:
REPOL Polypropylene C015EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol C015EG is recommended for use in blow molding and extrusion processes where high impact strength is required. It is an ideal material for making blow molded containers, sheets, automotive trims etc. Features: Consistent processabilityGood stiffness-impact balanceGood surface glossInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.5 MPa
3840 psi
50mm/min; ASTM D638
Elongation at Yield 11 %
11 %
50mm/min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% secant; ASTM D790A
Izod Impact, Notched 2.25 J/cm

@Temperature 23.0 °C
4.22 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648