Resin Technology Group H420 Oxy-Bond™ Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group H420 Oxy-Bond™ Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to match a variety of specific application parameters, including MIL-APPROVED. Custom designed bonding products and expert technical assistance are always available.Resin Technology Group H420 Oxy-Bond™ Electrically Conductive Epoxy AdhesiveFlexible two part room temperature curing silver conductive.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature >=110 °C
1.00 hour

@Temperature >=230 °F
120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
Pot Life 180 min
180 min
180 min
180 min
Descriptive Properties Value Comments
Viscosity Smooth Paste