Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.017 - 0.018 cm/cm

@Time 86400 sec
0.017 - 0.018 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.020 - 0.021 cm/cm

@Time 86400 sec
0.020 - 0.021 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527
89.0 MPa
12900 psi
ASTM D638
Elongation at Break 5.9 %
5.9 %
ASTM D638
6.3 %
6.3 %
ISO 527
Tensile Modulus 3.68 GPa
534 ksi
50 mm/min; ASTM D638
3.80 GPa
551 ksi
1 mm/min; ISO 527
Flexural Strength 107 MPa
15500 psi
ISO 178
131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ISO 178
3.93 GPa
570 ksi
ASTM D790
Izod Impact, Notched 0.460 J/cm
0.862 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.38
0.38
ASTM D3702 Modified
Coefficient of Friction, Static 0.32
0.32
ASTM D3702 Modified
K (wear) Factor 46.3 x 10-8 mm³/N-M
23.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 66.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
68.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 97.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
54.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
98.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
54.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 246 °C
475 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
171 °C

@Thickness 3.20 mm
340 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: