Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Tensile Modulus 6.62 GPa
960 ksi
50 mm/min; ASTM D638
Flexural Strength 172 MPa
24900 psi
ASTM D790
Flexural Modulus 6.59 GPa
956 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.18 J/cm
15.3 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 3.20 mm
289 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved