SABIC Innovative Plastics LNP THERMOCOMP ZX08309 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP ZX08309 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is mineral filled PPO grade with high dielectric constant and low loss tangent
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ASTM D955
Melt Index of Compound 11 g/10 min

@Load 5.00 kg,
Temperature 300 °C
11 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Flexural Strength 90.0 - 100 MPa
13100 - 14500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.20 - 3.50 GPa
464 - 508 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Dielectric Constant 4.4 - 4.6

@Frequency 1.00e+9 Hz
4.4 - 4.6

@Frequency 1.00e+9 Hz
ASTM ES 7-83
Dissipation Factor 0.0020 - 0.0040

@Frequency 1.10e+9 Hz
0.0020 - 0.0040

@Frequency 1.10e+9 Hz
ASTM ES 7-83