SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Impact Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on tensile bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 105 MPa
15200 psi
5 mm/min; ISO 527
Elongation at Yield >= 3.0 %
>= 3.0 %
5 mm/min; ISO 527
Tensile Modulus 4.90 GPa
711 ksi
1 mm/min; ISO 527
Flexural Strength 140 MPa
20300 psi
2 mm/min; ISO 178
Flexural Modulus 4.20 GPa
609 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
65.0 kJ/m²

@Temperature -30.0 °C
30.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af