SABIC Innovative Plastics NORYL PVX524 PPE

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PVX524 PPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT
Physical Properties Metric English Comments
Water Absorption at Saturation 0.060 %
0.060 %
ISO 62
Viscosity 110000 cP
110000 cP
Melt Viscosity, 280°C, 1500 sec-1; ISO 11443
Melt Index of Compound 24 g/10 min

@Load 5.00 kg,
Temperature 280 °C
24 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
50 mm/min; ISO 527
38.0 MPa
5510 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min; ISO 527
43.0 MPa
6240 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 32 %
32 %
Type I, 50 mm/min; ASTM D638
48 %
48 %
50 mm/min; ISO 527
Elongation at Yield 2.1 %
2.1 %
50 mm/min; ISO 527
2.3 %
2.3 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.34 GPa
339 ksi
1 mm/min; ISO 527
2.41 GPa
350 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 64.0 MPa
9280 psi
2 mm/min; ISO 178
66.0 MPa
9570 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.29 GPa
332 ksi
2 mm/min; ISO 178
2.46 GPa
357 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
0.940 J/cm

@Temperature -30.0 °C
1.76 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1A
8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact Unnotched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 6.00 J

@Temperature -40.0 °C
4.43 ft-lb

@Temperature -40.0 °F
ASTM D3763
17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C

@Thickness 3.20 mm
226 °F

@Thickness 0.126 in
unannealed; ASTM D648
111 °C

@Thickness 6.40 mm
232 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
93.0 °C

@Thickness 3.20 mm
199 °F

@Thickness 0.126 in
unannealed; ASTM D648
102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 113 °C
235 °F
Rate B/50; ASTM D1525