SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced tensile elongation, capable of VW-1 performance and 105C temperature rating as defined by UL 1581. 87 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0mm wire with 0.12mm X 20 stranded coppoer conductor.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 250 °C
16 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
30S reading; ASTM D2240
Tensile Strength at Break 16.0 MPa
2320 psi
Type I, 50 mm/min; ASTM D638
16.0 MPa
2320 psi
50 mm/min; ISO 527
26.0 MPa
3770 psi
after 7days @136°C; UL 1581
27.0 MPa
3920 psi
UL 1581
Elongation at Break 170 %
170 %
50 mm/min; ISO 527
180 %
180 %
Type I, 50 mm/min; ASTM D638
190 %
190 %
after 7days @136°C; UL 1581
250 %
250 %
UL 1581
Flexural Modulus 0.0400 GPa
5.80 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.0400 GPa
5.80 ksi
12.5 mm/min; ISO 178
Heat Distortion 10 %

@Load 0.250 kg,
Temperature 121 °C
10 %

@Load 0.551 lb,
Temperature 250 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 29 %
29 %
ISO 4589
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+17 ohm-cm
<= 1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 22.8 kV/mm

@Thickness 2.00 mm
579 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0035

@Frequency 1.00e+6 Hz
0.0035

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 146
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 112
ASTM E 662
VW-1 Pass
UL 1581