Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 300 °C
15 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 7.0 %
7.0 %
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 108 MPa
15700 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.27 GPa
764 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
22.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 51.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94 by SABIC-IP