Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Proâ„¢ P400S Polypropylene Flat Yarn/Sheet

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Pro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Proâ„¢ P400S Polypropylene Flat Yarn/Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:High outputGood mechanical propertiesRecommended Applications:Stretched tapeMonofilament for woven bag, woven sheet, rope, strap and sheetInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 500 hour

@Temperature 50.0 °C
>= 500 hour

@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D638
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
Izod Impact, Notched 0.167 J/cm

@Temperature -20.0 °C
0.312 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.245 J/cm

@Temperature 0.000 °C
0.459 ft-lb/in

@Temperature 32.0 °F
ASTM D256
0.392 J/cm

@Temperature 23.0 °C
0.735 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
ASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 50 %

@Thickness 1.00 mm
50 %

@Thickness 0.0394 in
ASTM D1003
Gloss 85 %

@Thickness 1.00 mm
85 %

@Thickness 0.0394 in
ASTM D2457
Users viewing this material also viewed the following: