Material Notes:
Application: A general purpose PVC based extrusion grade compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70.0

@Time 15.0 sec
70.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -22.0 °C
-7.60 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 171 - 177 °C
340 - 350 °F
Suggested Stock