SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Blow molded containers up to 30 liters for packagingChemicalsHousehold productsOils and foodstuffsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ISO 1872/1
ESCR, Bottle 25 hour

@Temperature 50.0 °C
25 hour

@Temperature 122 °F
BP 13C/25
Melt Flow 0.20 g/10 min

@Load 2.16 kg
0.20 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
BP 13B/1
Elongation at Break 1000 %
1000 %
BP 13B/1
Flexural Modulus 1.00 GPa
145 ksi
ISO 178-1975
Impact 3.3
3.3
M, F50; BP 13B/11