Material Notes:
Features and Applications: Compared with nylon 6 and nylon 66, nylon 610 is much softer and lower in water absorption, featured by excellent low temperature resistance and dimensional stability. Due to oil and chemicals resistance and excellent electric performance, it belongs to self-extinguishing material and can be applicable to coating of bristle like monofilaments of toothbrush and cables.Information provided by Shandong Guangyin
Physical Properties Metric English Comments
Density 1.07 - 1.13 g/cc
0.0387 - 0.0408 lb/in³
Viscosity Measurement 90 - 120
90 - 120
Type I
110 - 150
110 - 150
Type II
160 - 200
160 - 200
Type III
Evaporation Loss <= 1.0 %
<= 1.0 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 50.0 MPa
>= 7250 psi
Elongation at Break >= 100 %
>= 100 %
Flexural Strength >= 50.0 MPa
>= 7250 psi
Thermal Properties Metric English Comments
Melting Point 208 - 220 °C
406 - 428 °F
Descriptive Properties Value Comments
Granularity 30-50 N/g