Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Mar-Bal
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.90 - 2.00 g/cc
1.90 - 2.00 g/cc
ASTM D792
Bulk Factor 1.0
1.0
ASTM D1895
Filler Content 10 %
10 %
Glass
Water Absorption 0.17 %

@Time 86400 sec
0.17 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.00050 - 0.0030 cm/cm
0.00050 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 35 - 48
35 - 48
ASTM D2583
Tensile Strength 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D638
Flexural Strength 96.5 - 110 MPa
14000 - 16000 psi
ASTM D790
Flexural Modulus 13.8 - 15.2 GPa
2000 - 2200 ksi
ASTM D790
Compressive Strength 103 - 124 MPa
15000 - 18000 psi
ASTM D695
Shear Strength 41.4 - 48.3 MPa
6000 - 7000 psi
ASTM D732
Izod Impact, Notched 1.33 - 1.87 J/cm
2.50 - 3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Track Resistance 3000 sec
3000 sec
Inclined-Plane Tracking; ASTM D2303
Descriptive Properties Value Comments
Listed File E80533 No