Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Polidiemme® G/440 Thermoset Elastomer (TSE)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Polidiemme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polidiemme® G/440 Thermoset Elastomer (TSE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method)Standards complying: Cenelec HD 22.1 EI4, EI6, EI7 and EM3; EN 50363-0 G8; IEC 60502 EPR; IEC 60092/351 EPR; BS 7655 RS5 and GP7; VDE 0207/20 3GI3Features: Crosslinkable; Good Flexibility; Low ToxicityUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsAdditional Properties: Collar Temperature - 140 to 170 °C; Head Temperature - 140 to 170 °C; Hot Set - IEC 60811 50 %; Hot Set - IEC 60811 0.0 %; Hot Set - IEC 60811 70 %; Hot Set - IEC 60811 0.0 %; Insulation Resistance Constant - IEC 60502 (20°C): 15000 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 500 Mohm·km; Water Absorption - IEC 60811 (100°C): 1.00 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 0.882 g/cc
0.0319 lb/in³
ASTM D792
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 18
18
ISO 868
Tensile Strength at Break 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Tear Strength 3.50 kN/m
20.0 pli
ASTM D624
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+14 ohm-cm

@Temperature 90.0 °C
1.40e+14 ohm-cm

@Temperature 194 °F
ASTM D257
4.10e+15 ohm-cm

@Temperature 20.0 °C
4.10e+15 ohm-cm

@Temperature 68.0 °F
ASTM D257
Dielectric Constant 2.3

@Frequency 1000 Hz
2.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 32.0 kV/mm
813 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Zone 1 120 - 140 °C
248 - 284 °F
Zone 2 120 - 150 °C
248 - 302 °F
Zone 3 130 - 160 °C
266 - 320 °F
Zone 4 140 - 170 °C
284 - 338 °F
Die Cooling Temperature 140 - 170 °C
284 - 338 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant