Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two particle sizes to meet formulators' specific needs. Their inherent toughness imparts damage tolerance to thermoset composites. Virantage PESU polymers also offer superior thermal and hydrolytic stability that deliver best-in-class hot-wet performance. These amorphous thermoplastics may be used to toughen a variety of advanced thermoset composites used to produce high-performance aerospace components. Virantage PESU tougheners have been used successfully in a variety of thermosetting resin systems including epoxies, phenolics and BMIs. All Virantage PESU polymers are produced at Solvay's state-of-the-art, world-scale facility in Panoli, India under ISO 9001:2000 and ISO 14001:2004 certified quality management systems.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 1.0 %
1.0 %
Measured at time of packaging; Internal Method
Particle Size 63 µm
63 µm
VW-10300FP; D90 Particle sizes by sieve measurement
500 µm
500 µm
VW-10300P; D90 Particle sizes by sieve measurement
Viscosity 800 cP

@Temperature 40.0 °C
800 cP

@Temperature 104 °F
25% solution in DMAc; Internal Method
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 220 °C
428 °F
DSC
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Amorphous
Good Thermal Stability
Good Toughness
High Heat Resistance
Hydrolytically Stable
Medium Molecular Weight
Medium-high Viscosity
Forms Powder
Generic PESU
Processing Method Compounding
Residual Solvent (%) 0.2
Measured by Gas Chromatography
Uses Aerospace Applications