Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Mica Filler
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech PP5321 Mica Reinforced Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc

@Temperature 22.8 °C
1.08 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 25 %
25 %
Mica
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.4 MPa
4850 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 2.14 GPa
310 ksi
secant; ASTM D790
2.62 GPa
380 ksi
tangent; ASTM D790
Izod Impact, Notched 0.294 J/cm

@Temperature 22.8 °C
0.550 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D648
Users viewing this material also viewed the following: