Spartech SP-3810 TPO/TPE Polyolefin Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , TPO
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech SP-3810 TPO/TPE Polyolefin Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyolefin SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength at Break 15.9 MPa
2300 psi
ASTM D638
Elongation at Break 375 %
375 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Dart Drop 12.6 g/micron
320 g/mil
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 52.8 °C
127 °F
ASTM D648