Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet)
Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it..
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet)
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Quantum PEI - Ultem®
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Quantum Polysulfone
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Quantum PPSU
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
NOVA Chemicals Laboratory Procedure
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet)
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet)
CTE, linear 55.8 - 91.8 µm/m-°C
31.0 - 51.0 µin/in-°F
Average value: 69.2 µm/m-°C Grade Count:9
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products  (discontinued **)
ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and ..
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant
Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech SP-3810 TPO/TPE Polyolefin Sheet
Description: Polyolefin SheetInformation provided by Spartech.
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced
Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications
Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications
Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,..
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Westlake Plastics Radel® R Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Tempalux® Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Tempalux® Polyetherimide For Medical Applications
Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its ..
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications
Medical grade Zelux GS polycarbonate is produced from resin formulated to meet the stringent performance characteristics and requirements of the healthcare industry. Suitable for EtO gas and limite..
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Ensinger TECASON™ S Polysulfone (PSU)
TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD..
CTE, linear 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831