Sterigenics Raprex® R200D Branched High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Sterigenics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sterigenics Raprex® R200D Branched High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Injection Molding and ExtrusionRAPREX® R200D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched structure. It is a thermoplastic and is fully recyclable. Due to its high molecular weight and shear sensitivity, RAPREX® R200D is used for injection molding. Because of its high melt strength, it is also used for films, extrusion coating and foam applications. Raprex® R200D contains a robust stabilization package providing excellent melt stability as well as long-term heat aging.Information provided by Sterigenics
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Index of Compound 1.1 g/10 min

@Load 10.0 kg,
Temperature 190 °C
1.1 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.0 MPa
3050 psi
ASTM D638
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
2.60 J/cm

@Temperature -40.0 °C
4.87 ft-lb/in

@Temperature -40.0 °F
Partial Break; ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746