Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Novodur® BX13036 ABS + PMMA

Category Polymer , Thermoplastic , ABS Polymer , Acrylic (PMMA)
Manufacturer Styrolution
Trade Name Novodur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Novodur® BX13036 ABS + PMMA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
ISO 294-4
Melt Flow 16 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114.5
114.5
IEC 2039-2
Tensile Strength, Yield 48.0 MPa
6960 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Tensile Modulus 2.60 GPa
377 ksi
ISO 527
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 - 100 µm/m-°C
44.4 - 55.6 µin/in-°F
ISO 11359
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Vicat Softening Point 92.0 °C

@Load 5.10 kg
198 °F

@Load 11.2 lb
50°C/h; ISO 306
100 °C

@Load 1.02 kg
212 °F

@Load 2.25 lb
50°C/h; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+18 ohm-cm
>= 1.00e+18 ohm-cm
IEC 60093
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Melt Temperature 200 - 240 °C
392 - 464 °F
ISO 294
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
ISO 294
Drying Temperature 80.0 °C

@Time 7200 - 14400 sec
176 °F

@Time 2.00 - 4.00 hour
Users viewing this material also viewed the following: