Material Notes:
Characteristics Speciality grade containing silicon oil to provide wear resistance and high opacity jet black color Easy flowing grade Processing Injection moldingApplications Camera parts Photographic equipment parts Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.5 MPa
3550 psi
50 mm/min; ASTM D638
Elongation at Break 50 %
50 %
50 mm/min; ASTM D638
Flexural Strength 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.96 GPa

@Thickness 3.20 mm
284 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 3.20 mm
2.06 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Vicat Softening Point 99.0 °C
210 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F