Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Supreme Petrochem SP6433 9710 Medium Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Supreme Petrochem LTD
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Supreme Petrochem SP6433 9710 Medium Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics High flow Good toughness Good shine Available in various colors Processing Injection molding Extrusion Applications Pipes & profiles for wiring Beading for furniture and tables Containers for packaging Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 200 °C
17 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.4 MPa
4410 psi
50 mm/min; ASTM D638
Elongation at Break 35 %
35 %
50 mm/min; ASTM D638
Flexural Strength 49.0 MPa

@Thickness 3.20 mm
7110 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 2.21 GPa

@Thickness 3.20 mm
320 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.450 J/cm

@Thickness 3.20 mm
0.843 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Users viewing this material also viewed the following: