Material Notes:
Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistance, and superior adhesion strength with metal surfaces. It is widely used for coating of auto parts, hard wares, water pipes racks et al. Available in various colors to provide a customized product. It can be applied to subjects with a 0.7mm-0.3mm thickness range, and it can also achieve a thinner thickness when it is not coated by dipping. The optimal coating thickness is 0.12-0.15mm.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 0.90 %
0.90 %
ISO 62
Particle Size <= 80 µm
<= 80 µm
> 99 wt.%; DIN EN ISO 4610
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
ISO 868
Thermal Properties Metric English Comments
Melting Point 202 °C
396 °F
ISO 11357-3
Vicat Softening Point 186 °C
367 °F
ISO 306
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
ISO1210
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
ISO1210
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ISO 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ISO 60093
Descriptive Properties Value Comments
Salt Spray Resistance < 1mm corrosion
ISO 7253; Testing according to WIS 4-52-01; 2000 hours