Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 0650-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JC837DB Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Syncure™ System S112BL Polyethylene, Crosslinked (XLPE) Syncure™ systems are two part moisture crosslinkable compounds. S112BL is a CSA listed, high strength, weather resistant, black (2.5% carbon black) cable insulation compound. RoHS compliant.STORAGE.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D412 |
Polymax® Maxelast® P3890 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R7426A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R7543E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | 510 mm/min; ASTM D412A |
PolyOne Geon™ Vinyl Flexible XV3758 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PE 152 Polyethylene, Unspecified (PE, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PE126 BLK 3330 Polyethylene, Low Density (LDPE) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
ExxonMobil Escorene® LL-8361 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good flowUses: Consumer items, Potable water tanks, Laundry tubs |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi.. |
|||
Tensile Strength, Yield | 15.9 - 44.5 MPa | 2310 - 6450 psi | Average value: 28.5 MPa Grade Count:92 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2310 psi | ASTM D638 |
Resirene Resirene® 6110 High Impact Polystyrene Features:High ImpactEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityApplications:Injection MoldingTV CabinetsRemote ControlsToysInformation provided by US distributor Calsak Corporation. |