Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
5 seconds; ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D412
Elongation at Break 440 %
440 %
ASTM D412
100% Modulus 0.00565 GPa
0.820 ksi
ASTM D412
Tear Strength 52.6 kN/m
300 pli
ASTM D624
Compression Set 35 %
35 %
23°C, 22 hr.; ASTM D395, Method B
68 %
68 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746