Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® 4344 HDPE, blow molding  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® 4344 HDPE, blow molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: storage tank liners, intermediate bulk containers, general large-part blow molding. Blow Molding Stock Temperature 370 – 410 ºFInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
ASTM D1693 cond. B 100% lgepal
Melt Flow 0.34 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.34 g/10 min

@Load 11.0 lb,
Temperature 374 °F
High Load Melt Index 9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 22.8 MPa
>= 3300 psi
ASTM D 638 type IV
Elongation at Break >= 800 %
>= 800 %
ASTM D 638, type IV
Flexural Modulus 0.862 GPa
125 ksi
ASTM D 790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 126 °C
258 °F
ASTM D3417
Copyright © lookpolymers.com All Rights Reserved