Material Notes:
ATOFINA Polypropylene PPH 3051 is homopolymer.ApplicationATOFINA Polypropylene PPH 3051 is intended for the extrusion of flat bioriented films for food packaging or high strength adhesive tapes. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ISO 2039-2
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-2
Flexural Modulus 1.30 GPa
189 ksi
ISO 527-2
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C per hour; ISO 75-2
Vicat Softening Point 85.0 °C
185 °F
50N-50°C per hour; ISO 306
150 °C
302 °F
10N-50°C per hour; ISO 306