Tra-Con Tra-Bond Ablebond 868-7U Thixotropic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond Ablebond 868-7U Thixotropic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ablebond 868-7UNF is the unfilled version of 868-7, a nonsagging, flexible epoxy adhesive. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Adhesive Bond Strength 26.2 MPa
3800 psi
Lap shear, alum to alum
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 125 °C
0.500 hour

@Temperature 257 °F
60.0 min

@Temperature 75.0 °C
1.00 hour

@Temperature 167 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F