Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Duct 2924 Conductive Silver Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 2924 Conductive Silver Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage, low resistivity bonding applications where good electrical and physical properties over a wide temperature range (up to 190°C) are required. This smooth paste formulation of refined pure silver and epoxy is free of solvents and copper or carbon additives. It can be used -- after REQUIRED high temperature cure cycle -- for the assembly, manufacture and repair of electronic modules, printed circuits, integrated circuits, electrical contacts, capacitors, wave guides and flat cables, for high-frequency RF shieldings, and for applications where a "hot" soldering iron is impractical. Fully cured TRA-DUCT 2924 is a hard, dimensionally stable, conductive material which is resistant to water, weathering, gases and vapors, lubricants, fuels, alcohol, and also to those salts, salt solutions, mild acids and alkalis, and other organic and inorganic compounds with which silver itself is compatible. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.65 g/cc
2.65 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 25000 cP
25000 cP
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 8.76 MPa
1270 psi
Lap shear, alum to alum, 2 hrs @ 100°C
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C

@Temperature 20.0 °C
27.2 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 190 °C
374 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 92.0 °C
198 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.00020 ohm-cm
0.00020 ohm-cm
cured 2 hrs @ 125°C
0.00050 ohm-cm
0.00050 ohm-cm
cured 2 hrs @ 100°C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 125 °C
1.00 hour

@Temperature 257 °F
120 min

@Temperature 100 °C
2.00 hour

@Temperature 212 °F
Pot Life 240 min
240 min
Descriptive Properties Value Comments
Color Silver
Mix Ratio, parts by weight 100/5
Resin/Hardener