Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® 15 LV Variable Hardness Low Viscosity Catalyst

Category Polymer , Adhesive , Thermoset
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 15 LV Variable Hardness Low Viscosity Catalyst.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 15 LV Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. Long working life. Yields cured castings or adhesives having outstanding adhesion to a wide variety of substrates. Very low peak exotherm. Cure Type: Room Temp or Heat
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Viscosity 15000 cP

@Temperature 25.0 °C
15000 cP

@Temperature 77.0 °F
Mixed
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
960 - 1440 min

@Temperature 25.0 °C
16.0 - 24.0 hour

@Temperature 77.0 °F
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
100 grams
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: