Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Stycast® 1090/11 Two-Component General Purpose Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 1090/11 Two-Component General Purpose Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as well as thermal shock protection.Emerson & Cuming 1090/11 Stycast® Two-Component General Purpose EncapsulantGood Chemical ResistanceHigh temperatureMix Ratio by Weight = 100:10.5 Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 0.800 g/cc
0.0289 lb/in³
Viscosity 29000 cP

@Temperature 25.0 °C
29000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 155 °C
311 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.7

@Frequency 1e+6 Hz
2.7

@Frequency 1e+6 Hz
Dielectric Strength 14.8 kV/mm
375 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min
0.500 - 1.00 hour