Material Notes:
Made for injection molding applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 868
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ISO 306