High modulus and low warpage nylonInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.0 %
1.0 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.20 mm
0.0010 in/in

@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Thickness 3.20 mm
0.0050 in/in

@Thickness 0.126 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 129 MPa
18700 psi
ISO 527-1/-2
Elongation at Break 1.7 %
1.7 %
ISO 527-1/-2
Tensile Modulus 13.0 GPa
1890 ksi
ISO 527-1/-2
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 12.0 GPa
1740 ksi
ISO 178
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179-1
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-2