Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylon/Polypropylene AlloyInformation provided by Wellman.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.021 cm/cm
0.017 - 0.021 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-93
Elongation at Break 95 %
95 %
ISO 527-93
Flexural Strength 65.0 MPa
9430 psi
ISO 178-93
Flexural Modulus 1.75 GPa
254 ksi
ISO 178-93
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-93