Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.915 g/cc | 0.0331 lb/in³ | |
Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® FORMAX® L91507H Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Eastman 1390P Polyethylene
(discontinued **) Low-density polyethylene 1390P is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density polyethylen.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 800 Low Density Polyethylene
(discontinued **) IPETHENE® 800 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high flow and flexibility. APPLICATIONS IPETHENE® 800 i.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
LyondellBasell Montell 0300 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5021 400 Micron LDPE Powder Description: ICOFLO 510-5021 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5060 800 Micron LDPE Powder Description: ICOFLO 510-5060 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a barrier in ma.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5061 1200 Micron LDPE Powder Description: ICOFLO 510-5061 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5059 500 Micron LDPE Powder Description: ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Information provided by ICO Polymers.A Sch.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183 |
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183 |
Borealis CA9150 Low Density Polyethylene CA9150 is a low-density polyethylene for extrusion coating. CA9150 contains no additives. Applications: coating and lamination of aluminum foil, coating of various plastic films and cellophane, and.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D792 |
DuPont Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D792 |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake EC1390AA Low Density Polyethylene WESTLAKE low-density polyethylene EC1390 is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density po.. |
|||
Density | 0.915 g/cc @Temperature 15.6 °C |
0.0331 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exterex™ A51 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LD 202.48 Extrusion Coating Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade) Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Braskem PB 608 LDPE Injection Molding Polyethylene Description: PB608 is a grade produced under high pressure in an autoclave reactor. This grade is especially designed for injection molding of articles that must show excellent flexibility propertie.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM-D792 |
Braskem PCD 0140BR HECO Polypropylene Heterophasic Copolymer PCD 0140BR is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140BR is highly protected against thermal aging.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D-1505 |
Bapolene® 152F Polyethylene Film Grade Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 900 Low Density Polyethylene IPETHENE® 900 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high melt flow rate, good transparency, and flexibility. .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 600 Low Density Polyethylene IPETHENE® 600 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits good stiffness and moderate melt flow rate. APPLICATIONS.. |
|||
Density | 0.915 - 0.939 g/cc | 0.0331 - 0.0339 lb/in³ | Average value: 0.920 g/cc Grade Count:72 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D792 |
DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |