Westlake EP310 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EP310 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft goods packagingHigh clarity packagingBags for textile itemsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.9235 g/cc
0.03336 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 575 %
575 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Dart Drop 3.94 g/micron
100 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 23.4 MPa
3400 psi
ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
1% Secant Modulus, MD 186 MPa
27000 psi
ASTM D882
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 3.8 %
3.8 %
ASTM D1003
Gloss 80 %
80 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution