Material Notes:
Westlake MC3016 is a high density polyethylene designed for extrusion coating and lamination applications. MC3016 provides improved barrier properties, temperature resistance, stress crack resistance, scuff resistance, gloss and coefficient of friction (COF) compared to low density polyethylene.Application/UsesImaging paperRelease paperSpiral wound can liningsGrease barrierFDA: This material complies with FDA regulations in 21 CFR, section 177.1520.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.1 MPa
3210 psi
500mm/min; ASTM D638
Elongation at Break 20 %
20 %
500mm/min; ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Descriptive Properties Value Comments
Process Coating
Users viewing this material also viewed the following: