Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy

Category Polymer , Thermoplastic
Manufacturer Wolf Kunststoff
Trade Name ZEDEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Main Characteristics: Tough; Resilient; Soft; Low cost solutionApplications: Handling, Vessel and pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided by Zedex
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 50.0 MPa
7250 psi
Flexural Strength 70.0 MPa
10200 psi
Fatigue Strength 40.0 MPa
5800 psi
K Factor (ISO) 0.44 µm/km
0.44 µm/km
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 55.0 °C
131 °F
Continuous
75.0 °C
167 °F
Short Term (3h)
Minimum Service Temperature, Air -100 °C
-148 °F
Continuous
Electrical Properties Metric English Comments
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Descriptive Properties Value Comments
Sliding Velocity 40