Material Notes:
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
GB-1033
Mechanical Properties Metric English Comments
Tensile Strength, Yield 74.0 MPa
10700 psi
GB-1040
Elongation at Break 3.0 %
3.0 %
GB-1040
Flexural Strength 119.5 MPa
17330 psi
GB-9341
Flexural Modulus 5.00 GPa
725 ksi
GB-9341
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
GB-1043
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 192 °C
378 °F
GB-1634
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
GB-1410
Comparative Tracking Index 550 V
550 V
GB4207
Processing Properties Metric English Comments
Processing Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 110 - 120 °C

@Time 14400 - 18000 sec
230 - 248 °F

@Time 4.00 - 5.00 hour
Injection Pressure 80.0 - 120 MPa
11600 - 17400 psi