Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell BT-33 Nylon 6, 15% Glass Reinforced; Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell BT-33 Nylon 6, 15% Glass Reinforced; Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0075 cm/cm
0.0075 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 78
78
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 93.1 MPa
13500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.10 GPa
595 ksi
ASTM D790
Compressive Yield Strength 97.0 MPa
14100 psi
ASTM D695
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 199 °C
390 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Flammability, UL94 HB
HB