| Category | Polymer , Thermoplastic , Elastomer, TPE , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS) |
| Manufacturer | Polykemi AB |
| Trade Name | POLYelast |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
| 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 @Time 15.0 sec |
60 @Time 0.00417 hour |
Polykemi |
| Tensile Strength at Break | <= 6.50 MPa | <= 943 psi | ISO/R527 |
| Elongation at Break | 650 % | 650 % | ISO/R527 |
| 100% Modulus | 0.00130 GPa | 0.189 ksi | ISO/R527 |
| 300% Modulus | 0.00220 GPa | 0.319 ksi | ISO/R527 |
| Compression Set | 20 % @Temperature 23.0 °C, Time 259000 sec |
20 % @Temperature 73.4 °F, Time 72.0 hour |
DIN 53517 |
| 75 % @Temperature 70.0 °C, Time 86400 sec |
75 % @Temperature 158 °F, Time 24.0 hour |
DIN 53517 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | Low | % of injection pressure |
| Injection Pressure | Low | |
| Injection Speed () | High |