Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20000 - 80000 cP | 20000 - 80000 cP | |
Lord Adhesives 206 Long Working Time Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Viscosity | 10000 - 80000 cP | 10000 - 80000 cP | Hardener |
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic AdhesiveLord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to m.. |
|||
Viscosity | 50000 - 80000 cP | 50000 - 80000 cP | B |
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works. |
|||
Viscosity | 50000 - 80000 cP | 50000 - 80000 cP | B |
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide.. |
|||
Viscosity | 50000 - 80000 cP | 50000 - 80000 cP | B |
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo.. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U0351C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U1753C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | ASTM D803 |
SK Chemicals SKYTHANE® US130J Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 70000 - 80000 cP | 70000 - 80000 cP | |
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl.. |
|||
Viscosity | 60000 - 80000 cP | 60000 - 80000 cP | |
Master Bond LED401LV One Component, Moderate Viscosity LED Curable System Master Bond LED401LV is a very special, one part LED type system that will cure when exposed to a light source emitting 405 nm wavelength and where the presence of any UV light is minimal or inciden.. |
|||
Viscosity | 70000 - 80000 cP @Temperature 23.0 °C |
70000 - 80000 cP @Temperature 73.4 °F |
|
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound Master Bond Polymer System EP21TDC-2 is a two component highly flexible epoxy resin compound for high performance bonding, sealing, coating and encapsulation. It is formulated to cure fully at ambie.. |
|||
Viscosity | 70000 - 80000 cP @Temperature 23.0 °C |
70000 - 80000 cP @Temperature 73.4 °F |
|
Master Bond EP34 Room Temperature Curing Two Component Epoxy System Master Bond Polymer System EP34 is a unique room temperature curing two component epoxy compound for high temperature potting and encapsulating applications. Adhesion to metals, glass, ceramics, woo.. |
|||
Viscosity | 70000 - 80000 cP @Temperature 23.0 °C |
70000 - 80000 cP @Temperature 73.4 °F |
|
Master Bond EP35 High Temperature Resistant Two Component Epoxy System Master Bond Polymer Adhesive EP35 is a unique, room temperature curing, two component epoxy adhesive for high temperature bonding applications. Master Bond Polymer Adhesive EP35 produces high stren.. |
|||
Viscosity | 20000 - 80000 cP | 20000 - 80000 cP | dynamic |
Dow Corning Q2-7406 ADHESIVE Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning |
|||
Viscosity | 30000 - 80000 cP | 30000 - 80000 cP | dynamic |
Dow Corning Q2-7735 ADHESIVE Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | |
3M Scotch-Weld™ EC-1469 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | |
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 60000 - 80000 cP | 60000 - 80000 cP | |
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C) |
|||
Viscosity | 24000 - 80000 cP | 24000 - 80000 cP | Thixotropic |
Loctite® 577 Coarse Threads Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |