| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
|
PolyOne OnForce™ LFT NN-60LGF/000 HS UV Black Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1/1eU |
|
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data)
Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
|
Pasargad Polymer Peyvand Pasamid 3P-H7130B Nylon 6/66, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | flatwise; ISO 179 1fU |
|
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 50-0957 Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | |
|
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature -30.0 °C
|
38.1
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned
Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America ..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179 |
|
Ter Hell Plastic Terez® PA 6 7500 TF 20 GF 20 Polyamide 6, 20% PTFE chemically bonded 20% glass fiber reinforced
Description: Medium viscosity PA 6, 20% PTFE chemically bonded and 20% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
|
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Conditioned
Information provided by Unitika Ltd.
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 30.0 °C
|
38.1
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30
Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p..
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 30.0 °C
|
38.1
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30
Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® GM-4H PA*-MD40
Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G..
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 30.0 °C
|
38.1
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50
Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30
Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30
Information provided by EMS Grivory
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 30.0 °C
|
38.1
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TSG-50/4 PA666-GF50
Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TSGZ-25/4 PA666-GF25
Information provided by EMS Grivory
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® TSGZ-30 PA666-GF30
Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40
Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate..
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature -30.0 °C
|
38.1
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50
Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
|
|||
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179 1eU |
|
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature -30.0 °C
|
38.1
ft-lb/in² <br>@Temperature -22.0 °F
|
|
|
BASF Polystyrol® 454 C Impact Grade Polystyrene (Europe)
Easy flowing, medium-impact grade.Data was collected by ISO methods and provided by BASF.
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 23.0 °C
|
38.1
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 30.0 °C
|
38.1
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50
Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature 30.0 °C
|
38.1
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TS FR PA666 FR
Information provided by EMS Grivory
|
|||
| Charpy Impact Unnotched |
8.00
J/cm² <br>@Temperature -30.0 °C
|
38.1
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Dry)
Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness.
|
|||