| Category | Polymer , Thermoplastic , Nylon , Nylon 610 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® RS |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.16 g/cc | 0.0419 lb/in³ | |
| 1.31 g/cc | 0.0473 lb/in³ | DAM; ISO 1183 | |
| Moisture Absorption | 1.20 % @Thickness 2.00 mm |
1.20 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity | 360000 cP @Temperature 250 °C |
360000 cP @Temperature 482 °F |
DAM; @ 1000 sec-1; ISO 11443 |
| 94180 cP @Shear Rate 5000 1/s, Temperature 280 °C |
94180 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| 116100 cP @Shear Rate 5000 1/s, Temperature 260 °C |
116100 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 | |
| 130300 cP @Shear Rate 5000 1/s, Temperature 250 °C |
130300 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 | |
| 341600 cP @Shear Rate 500 1/s, Temperature 280 °C |
341600 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| 455400 cP @Shear Rate 500 1/s, Temperature 260 °C |
455400 cP @Shear Rate 500 1/s, Temperature 500 °F |
ISO 11403-1 -2 | |
| 527100 cP @Shear Rate 500 1/s, Temperature 250 °C |
527100 cP @Shear Rate 500 1/s, Temperature 482 °F |
ISO 11403-1 -2 | |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 130 MPa | 18900 psi | 50%RH; ISO 527-1/-2 |
| 140 MPa | 20300 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 3.6 % | 3.6 % | DAM; ISO 527-1/-2 |
| 6.5 % | 6.5 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 6.80 GPa | 986 ksi | 50%RH; ISO 527-1/-2 |
| 8.10 GPa | 1170 ksi | DAM; ISO 527-1/-2 | |
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | DAM; ISO 180/1A |
| 16.0 kJ/m² | 7.61 ft-lb/in² | 50%RH; ISO 180/1A | |
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | DAM; ISO 179/1eU |
| 9.50 J/cm² | 45.2 ft-lb/in² | 50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | DAM; ISO 179/1eA |
| 1.50 J/cm² | 7.14 ft-lb/in² | 50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 2.28 J/g-°C | 0.545 BTU/lb-°F | |
| Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | of melt |
| Melting Point | 225 °C | 437 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 207 °C | 405 °F | DAM; ISO 75-1/-2 |
| Glass Transition Temp, Tg | 50.0 °C | 122 °F | DAM; 10°C/min; ISO 11357-1/-2 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additives | Lubricants | |
| Release agent | ||
| Delivery Form | Pellets | |
| Part Marking Code | >PA610-GF30< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | PA610-GF30 | ISO 1043 |
| Special Characteristics | Heat stabilised or stable to heat |