| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded |
| Manufacturer | Styrolution |
| Trade Name | Terlux® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Styrolution Terlux® 2802 TR MABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Water Absorption | 0.70 % | 0.70 % | ISO 62 |
| Moisture Absorption at Equilibrium | 0.35 % | 0.35 % | 23°C/50% R.H.; ISO 62 |
| Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
| Melt Flow | 2.0 g/10 min @Temperature 200 °C |
2.0 g/10 min @Temperature 392 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 48.0 MPa | 6960 psi | 50mm/min; ISO 527 |
| 48.0 MPa | 6960 psi | 2 in/min; ASTM Test | |
| Elongation at Break | 12 % | 12 % | 50mm/min, Nominal strain; ISO 527 |
| Elongation at Yield | 4.0 % | 4.0 % | 50mm/min; ISO 527 |
| Tensile Modulus | 2.00 GPa | 290 ksi | 1mm/min; ISO 527 |
| 2.00 GPa | 290 ksi | ASTM Test | |
| Izod Impact, Notched | 0.690 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM Test |
| Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO 179 |
| 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 | |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 |
| 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359 |
| Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | annealed; ASTM Test |
| 94.0 °C | 201 °F | ISO 75 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | annealed; ASTM Test |
| 90.0 °C | 194 °F | ISO 75 | |
| Vicat Softening Point | 91.0 °C | 196 °F | Rate "A" Loading 1 (50 degC/h 10N); ASTM Test |
| 93.0 °C | 199 °F | (50 °C/h / 50N) - B/50; ISO 306 | |
| Glass Transition Temp, Tg | 107 °C | 225 °F | 10 K/min; ISO 11357-1/-3 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 80 % | 80 % | unknown thickness |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Dielectric Constant | 2.8 @Frequency 1.00e+6 Hz |
2.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.9 @Frequency 100 Hz |
2.9 @Frequency 100 Hz |
IEC 60250 | |
| Dissipation Factor | 0.014 @Frequency 1.00e+6 Hz |
0.014 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 0.016 @Frequency 100 Hz |
0.016 @Frequency 100 Hz |
IEC 60250 | |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 229 - 260 °C | 444 - 500 °F | Injection Molding |
| 250 °C | 482 °F | Injection molding | |
| Mold Temperature | 48.9 - 73.9 °C | 120 - 165 °F | Injection Molding |
| 90.0 °C | 194 °F | Ejection temperature | |
| Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
| Drying Temperature | 70.0 °C | 158 °F | Injection Molding |
| Dry Time | 2 - 4 hour | 2 - 4 hour | Injection Molding |
| Moisture Content | 0.70 % | 0.70 % | ASTM Data |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Clear | |
| Commercial Status | North America and Europe | |
| Impact Modified | Yes | |
| Injection Molding Regrind | <10% | |
| NSF Std. 51 | No | |
| NSF Std. 61 | No | |
| Primary Processing Technique | Injection Molding | |
| Processing | Blow Molding | |
| Film Extrusion | ||
| Injection Molding | ||
| Profile Extrusion | ||
| Sheet Extrusion | ||
| Thermoforming | ||
| Special characteristic | Platable | |
| UL.UL-C | Yes |