Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 435 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 142 - 224 °C
288 - 435 °F
Average value: 207 °C Grade Count:25
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Melting Point 212 - 224 °C
414 - 435 °F
Average value: 216 °C Grade Count:29
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Melting Point 220 - 224 °C
428 - 435 °F
ASTM DSC
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, 50% RH
Neat resin, for compounding.Information provided by Cresset Powers Ltd.
Melting Point 220 - 224 °C
428 - 435 °F
ASTM DSC
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, Dry As Molded
Neat resin, for compounding.Information provided by Cresset Powers Ltd.
Melting Point 220 - 224 °C
428 - 435 °F
ASTM DSC
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, 50% RH
Neat resin, for compounding.Information provided by Cresset Powers Ltd.
Melting Point 220 - 224 °C
428 - 435 °F
ASTM DSC
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded
Neat resin, for compounding.Information provided by Cresset Powers Ltd.
Melting Point 156 - 224 °C
313 - 435 °F
Average value: 203 °C Grade Count:93
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..