Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
<br>@Temperature 65.6 °C
0.280 BTU/lb-°F
<br>@Temperature 150 °F
ASTM C351
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Specific Heat Capacity 1.17 J/g-°C
<br>@Temperature 70.0 °C
0.280 BTU/lb-°F
<br>@Temperature 158 °F
ASTM D648
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. ..
Specific Heat Capacity 1.17 - 1.81 J/g-°C
<br>@Temperature 50.0 - 200 °C
0.280 - 0.433 BTU/lb-°F
<br>@Temperature 122 - 392 °F
Average value: 1.51 J/g-°C Grade Count:6
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
ASTM D2766
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® 823 Polyester Film, 48 Gauge
Mylar® 823 is a two side, differentially pretreated, polyester film designed to provide excellent adhesion in print and lamination applications.Approvals: FDA Food Contact Status - All gauges of My..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge
Mylar® 840 is a one-side pretreated polyester film for improved metal or cold seal adhesion. The packaging industry is constantly setting higher standards for product protection using flexible pack..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge
Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® CL Polyester Film, 50 Gauge
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® E Polyester Film, 142 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® EL Polyester Film, 200 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® EL21 Polyester Film, 1400 Gauge
Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® LBTW Polyester Film, 48 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® LBTW Polyester Film, 92 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® OWF Polyester Film, 80 Gauge
Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® RB43 Polyester Film, 100 Gauge
Mylar® RB43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite side. Mylar® R..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® RL31 Polyester Film, 50 Gauge
Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® RSX951 Polyester Film, 92 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 284 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® HR951 Polyester Film, 92 Gauge
Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont.
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® MDA Polyester Film, 142 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge
Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Heat Capacity 1.17 - 1.51 J/g-°C
0.280 - 0.360 BTU/lb-°F
DSC
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Copyright © lookpolymers.com All Rights Reserved